Czech
Albanian
Arabic
Armenian
Azerbaijani
Belarusian
Bengali
Bosnian
Catalan
Czech
Danish
Deutsch
Dutch
English
Estonian
Finnish
Français
Greek
Haitian Creole
Hebrew
Hindi
Hungarian
Icelandic
Indonesian
Irish
Italian
Japanese
Korean
Latvian
Lithuanian
Macedonian
Mongolian
Norwegian
Persian
Polish
Portuguese
Romanian
Russian
Serbian
Slovak
Slovenian
Spanish
Swahili
Swedish
Turkish
Ukrainian
Vietnamese
Български
中文(简体)
中文(繁體)
Brazilian oral research

Papain-based gel for biochemical caries removal: influence on microtensile bond strength to dentin.

Články mohou překládat pouze registrovaní uživatelé
Přihlášení Registrace
Odkaz je uložen do schránky
Evandro Piva
Fabrício Aulo Ogliari
Rafael Ratto de Moraes
Felipe Corá
Sandrina Henn
Lourenço Correr-Sobrinho

Klíčová slova

Abstraktní

This study investigated the influence of a papain-based gel (Papacárie) for chemo-mechanical caries removal on bond strength to dentin. Human molars were assigned to the following groups: Group 1: sound teeth were flattened to expose dentin; Group 2: after flattening of surfaces, the papain-based gel was applied on the sound dentin; Group 3: overlying enamel from carious teeth was removed and mechanical excavation of dentin was conducted; Group 4: chemo-mechanical excavation of carious dentin was conducted using the papain-based gel. The Prime&Bond NT or Clearfil SE Bond adhesive systems were used for restorative procedures. A microtensile bond strength test was performed, and the modes of failure were determined under SEM. The data were submitted to two-way ANOVA and Tukey's test (p < or = 0.05). No significant differences were observed between the sound dentin groups. For both excavation methods, Clearfil presented a significantly higher bond strength than Prime&Bond NT. Also, for Clearfil, the mechanically excavated samples disclosed a significantly higher bond strength than the chemo-mechanically ones. For Prime&Bond NT, no significant differences were detected between the excavation methods. Predominance of mixed failures for the sound substrate and of adhesive failures for the carious dentin one was detected. The bond strength to carious dentin of the self-etching system was negatively affected by chemo-mechanical excavation using the papain-based gel.

Připojte se k naší
facebookové stránce

Nejúplnější databáze léčivých bylin podložená vědou

  • Funguje v 55 jazycích
  • Bylinné léky podporované vědou
  • Rozpoznávání bylin podle obrázku
  • Interaktivní mapa GPS - označte byliny na místě (již brzy)
  • Přečtěte si vědecké publikace související s vaším hledáním
  • Hledejte léčivé byliny podle jejich účinků
  • Uspořádejte své zájmy a držte krok s novinkami, klinickými testy a patenty

Zadejte symptom nebo chorobu a přečtěte si o bylinách, které by vám mohly pomoci, napište bylinu a podívejte se na nemoci a příznaky, proti kterým se používá.
* Všechny informace vycházejí z publikovaného vědeckého výzkumu

Google Play badgeApp Store badge