Czech
Albanian
Arabic
Armenian
Azerbaijani
Belarusian
Bengali
Bosnian
Catalan
Czech
Danish
Deutsch
Dutch
English
Estonian
Finnish
Français
Greek
Haitian Creole
Hebrew
Hindi
Hungarian
Icelandic
Indonesian
Irish
Italian
Japanese
Korean
Latvian
Lithuanian
Macedonian
Mongolian
Norwegian
Persian
Polish
Portuguese
Romanian
Russian
Serbian
Slovak
Slovenian
Spanish
Swahili
Swedish
Turkish
Ukrainian
Vietnamese
Български
中文(简体)
中文(繁體)
Heliyon 2020-Feb

Marginal integrity of aesthetic restorations following intracoronal bleaching with sweet potato extract as an additive: An SEM study.

Články mohou překládat pouze registrovaní uživatelé
Přihlášení Registrace
Odkaz je uložen do schránky
Gurucharan Ishwarya
Sampath Vidhya
Sekar Mahalaxmi

Klíčová slova

Abstraktní

The aim of this in vitro study was to evaluate the marginal integrity of an alkasite restoration in comparison to that of a conventional composite resin restoration following intra-coronal bleaching with 30% hydrogen peroxide (HP) containing sweet potato extract (SPE) as an additive. Access cavities were prepared in 60 extracted human incisors. The teeth were decoronated 2mm below the CEJ and the pulp chambers were sealed cervically. The samples were divided into two groups (n = 30) based on the type of restorative material - group I: Hybrid composite resin and group II: Alkasite restorative material. Both the groups were divided into three subgroups (n = 10) based on the intra-coronal bleaching agent used namely, subgroup A: no bleaching (NB); subgroup B: 30% hydrogen peroxide (HP) and subgroup C: 30% hydrogen peroxide containing SPE (HSP). The tooth-restorative interface was observed under a scanning electron microscope (SEM) to determine the marginal integrity. The results were tabulated and statistically analyzed using one-way ANOVA. Specimens bleached with HP alone showed higher marginal gaps, irrespective of the restorative material used. Subgroups A and C showed lesser marginal gaps under both the restorative materials. An improved marginal integrity was seen with the alkasite material. It can be concluded that the addition of SPE to HP improves the marginal integrity of the coronal restorative material placed immediately post-bleaching. The new alkasite material holds promise as a permanent coronal seal in cases of intra-coronal bleaching.

Připojte se k naší
facebookové stránce

Nejúplnější databáze léčivých bylin podložená vědou

  • Funguje v 55 jazycích
  • Bylinné léky podporované vědou
  • Rozpoznávání bylin podle obrázku
  • Interaktivní mapa GPS - označte byliny na místě (již brzy)
  • Přečtěte si vědecké publikace související s vaším hledáním
  • Hledejte léčivé byliny podle jejich účinků
  • Uspořádejte své zájmy a držte krok s novinkami, klinickými testy a patenty

Zadejte symptom nebo chorobu a přečtěte si o bylinách, které by vám mohly pomoci, napište bylinu a podívejte se na nemoci a příznaky, proti kterým se používá.
* Všechny informace vycházejí z publikovaného vědeckého výzkumu

Google Play badgeApp Store badge