English
Albanian
Arabic
Armenian
Azerbaijani
Belarusian
Bengali
Bosnian
Catalan
Czech
Danish
Deutsch
Dutch
English
Estonian
Finnish
Français
Greek
Haitian Creole
Hebrew
Hindi
Hungarian
Icelandic
Indonesian
Irish
Italian
Japanese
Korean
Latvian
Lithuanian
Macedonian
Mongolian
Norwegian
Persian
Polish
Portuguese
Romanian
Russian
Serbian
Slovak
Slovenian
Spanish
Swahili
Swedish
Turkish
Ukrainian
Vietnamese
Български
中文(简体)
中文(繁體)
Polymers 2020-Aug

Development of Thermoplastic Starch (TPS) Including Leather Waste Fragments

Only registered users can translate articles
Log In/Sign up
The link is saved to the clipboard
Silvio Pompei
Jacopo Tirillò
Fabrizio Sarasini
Carlo Santulli

Keywords

Abstract

A thermoplastic starch (TPS) material is developed, based on corn starch plasticized with glycerol and citric acid in a 9:3:1 ratio and further bonded with isinglass and mono- and diglycerides of fatty acids (E471). In TPS, leather fragments, in the amount of 7.5 15 or 22.5 g/100 g of dry matter, were also introduced. The mixture was heated at a maximum temperature of 80 °C, then cast in an open mold to obtain films with thickness in the range 300 ± 50 microns. The leather fragments used were based on collagen obtained from production waste from shoemaking and tanned with tannins obtained from smoketree (Rhus cotinus), therefore free from chromium. Thermogravimetric (TGA) tests suggested that material degradation started at a temperature around 285 °C, revealing that the presence of leather fragments did not influence the occurrence of this process in TPS. Tensile tests indicated an increase in tensile properties (strength and Young's modulus) with increasing leather content, albeit coupled, especially at 22.5 wt%, with a more pronounced brittle behavior. Leather waste provided a sound interface with the bulk of the composite, as observed under scanning electron microscopy. The production process indicated a very limited degradation of the material after exposure to UV radiation for eight days, as demonstrated by the slight attenuation of amide I (collagen) and polysaccharide FTIR peaks. Reheating at 80 °C resulted in a weight loss not exceeding 3%.

Keywords: leather waste; mechanical characterization; thermal characterization; thermoplastic starch.

Join our facebook page

The most complete medicinal herbs database backed by science

  • Works in 55 languages
  • Herbal cures backed by science
  • Herbs recognition by image
  • Interactive GPS map - tag herbs on location (coming soon)
  • Read scientific publications related to your search
  • Search medicinal herbs by their effects
  • Organize your interests and stay up do date with the news research, clinical trials and patents

Type a symptom or a disease and read about herbs that might help, type a herb and see diseases and symptoms it is used against.
*All information is based on published scientific research

Google Play badgeApp Store badge