Albanian
Arabic
Armenian
Azerbaijani
Belarusian
Bengali
Bosnian
Catalan
Czech
Danish
Deutsch
Dutch
English
Estonian
Finnish
Français
Greek
Haitian Creole
Hebrew
Hindi
Hungarian
Icelandic
Indonesian
Irish
Italian
Japanese
Korean
Latvian
Lithuanian
Macedonian
Mongolian
Norwegian
Persian
Polish
Portuguese
Romanian
Russian
Serbian
Slovak
Slovenian
Spanish
Swahili
Swedish
Turkish
Ukrainian
Vietnamese
Български
中文(简体)
中文(繁體)
Applied Spectroscopy 2010-Sep

Characterization of fungal-degraded lime wood by X-ray diffraction and cross-polarization magic-angle-spinning 13C-nuclear magnetic resonance spectroscopy.

Samo registrirani korisnici mogu prevoditi članke
Prijava Registriraj se
Veza se sprema u međuspremnik
Carmen-Mihaela Popescu
Per Tomas Larsson
Carmen Mihaela Tibirna
Cornelia Vasile

Ključne riječi

Sažetak

X-ray diffraction, scanning electron microscopy (SEM), and solid-state cross-polarization magic-angle-spinning (CP/MAS) (13)C-NMR spectroscopy were applied to determine changes over time in the morphology and crystallinity of lime wood (Tilia cordata Miller) generated by the soft-rot fungi. Wood samples were inoculated with Trichoderma viride Pers for various durations up to 84 days. Structural and morphological modifications were assessed by comparing the structural features of decayed lime wood samples with references. Significant morphology changes such as defibration or small cavities were clearly observed on the SEM micrographs of lime wood samples exposed to fungi. Following the deconvolution process of the diffraction patterns, the degree of crystallinity, apparent lateral crystallite size, the proportion of crystallite interior chains, and the cellulose fraction have been determined. It was found that all crystallographic data vary with the duration of exposure to fungi. The degree of crystallinity and cellulose fraction tend to decrease, whereas the apparent lateral crystallite size and the proportion of crystallite interior chains increase with prolonged biodegradation processes. The most relevant signals in CP/MAS (13)C-NMR spectra were assigned according to literature data. The differences observed were discussed in terms of lignin and cellulose composition: by fixing the lignin reference signal intensity, the cellulose and hemicelluloses moieties showed a relative decrease compared to the lignin signals in decayed wood.

Pridružite se našoj
facebook stranici

Najkompletnija baza ljekovitog bilja potpomognuta znanošću

  • Radi na 55 jezika
  • Biljni lijekovi potpomognuti znanošću
  • Prepoznavanje bilja slikom
  • Interaktivna GPS karta - označite bilje na mjestu (uskoro)
  • Pročitajte znanstvene publikacije povezane s vašom pretragom
  • Pretražite ljekovito bilje po učincima
  • Organizirajte svoje interese i budite u toku s istraživanjem vijesti, kliničkim ispitivanjima i patentima

Upišite simptom ili bolest i pročitajte o biljkama koje bi mogle pomoći, unesite travu i pogledajte bolesti i simptome protiv kojih se koristi.
* Svi podaci temelje se na objavljenim znanstvenim istraživanjima

Google Play badgeApp Store badge