Icelandic
Albanian
Arabic
Armenian
Azerbaijani
Belarusian
Bengali
Bosnian
Catalan
Czech
Danish
Deutsch
Dutch
English
Estonian
Finnish
Français
Greek
Haitian Creole
Hebrew
Hindi
Hungarian
Icelandic
Indonesian
Irish
Italian
Japanese
Korean
Latvian
Lithuanian
Macedonian
Mongolian
Norwegian
Persian
Polish
Portuguese
Romanian
Russian
Serbian
Slovak
Slovenian
Spanish
Swahili
Swedish
Turkish
Ukrainian
Vietnamese
Български
中文(简体)
中文(繁體)
Optics Express 2012-Jun

Linkage of oxygen deficiency defects and rare earth concentrations in silica glass optical fiber probed by ultraviolet absorption and laser excitation spectroscopy.

Aðeins skráðir notendur geta þýtt greinar
Skráðu þig / skráðu þig
Krækjan er vistuð á klemmuspjaldið
Y-S Liu
T C Galvin
T Hawkins
J Ballato
L Dong
P R Foy
P D Dragic
J G Eden

Lykilorð

Útdráttur

Ultraviolet absorption measurements and laser excitation spectroscopy in the vicinity of 248 nm provide compelling evidence for linkages between the oxygen deficiency center (ODC) and rare earth concentrations in Yb and Er-doped glass optical fibers. Investigations of YAG-derived and solution-doped glass fibers are described. For both Yb and Er-doped fibers, the dependence of Type II ODC absorption on the rare earth number density is approximately linear, but the magnitude of the effect is greater for Yb-doped fibers. Furthermore, laser excitation spectra demonstrate unambiguously the existence of an energy transfer mechanism coupling an ODC with Yb(3+). Photopumping glass fibers with a Ti:sapphire laser/optical parametric amplifier system, tunable over the 225-265 nm region, or with a KrF laser at 248.4 nm show: 1) emission features in the 200-1100 nm interval attributable only to the ODC (Type II) defect or Yb(3+), and 2) the excitation spectra for ODC (II) emission at ~280 nm and Yb(3+) fluorescence (λ ~1.03 μm) to be, within experimental uncertainty, identical. The latter demonstrates that, when irradiating Yb-doped silica fibers between ~240 and 255 nm, the ODC (II) defect is at least the primary precursor to Yb(3+) emission. Consistent with previous reports in the literature, the data show the ODC (II) absorption spectrum to have a peak wavelength and breadth of ~246 nm and ~19 nm (FWHM). Experiments also reveal that, in the absence of Yb, incorporating either Al(2)O(3) or Y(2)O(3) into glass fibers has a negligible impact on the ODC concentration. Not only do the data reported here demonstrate the relationship between the ODC (II) number density and the Yb doping concentration, but they also suggest that the appearance of ODC defects in the fiber is associated with the introduction of Yb and the process by which the fiber is formed.

Skráðu þig á
facebook síðu okkar

Heillasta gagnagrunnur lækningajurtanna sem studdur er af vísindum

  • Virkar á 55 tungumálum
  • Jurtalækningar studdir af vísindum
  • Jurtaviðurkenning eftir ímynd
  • Gagnvirkt GPS kort - merktu jurtir á staðsetningu (kemur fljótlega)
  • Lestu vísindarit sem tengjast leit þinni
  • Leitaðu að lækningajurtum eftir áhrifum þeirra
  • Skipuleggðu áhugamál þitt og vertu vakandi með fréttarannsóknum, klínískum rannsóknum og einkaleyfum

Sláðu inn einkenni eða sjúkdóm og lestu um jurtir sem gætu hjálpað, sláðu jurt og sjáðu sjúkdóma og einkenni sem hún er notuð við.
* Allar upplýsingar eru byggðar á birtum vísindarannsóknum

Google Play badgeApp Store badge