Lithuanian
Albanian
Arabic
Armenian
Azerbaijani
Belarusian
Bengali
Bosnian
Catalan
Czech
Danish
Deutsch
Dutch
English
Estonian
Finnish
Français
Greek
Haitian Creole
Hebrew
Hindi
Hungarian
Icelandic
Indonesian
Irish
Italian
Japanese
Korean
Latvian
Lithuanian
Macedonian
Mongolian
Norwegian
Persian
Polish
Portuguese
Romanian
Russian
Serbian
Slovak
Slovenian
Spanish
Swahili
Swedish
Turkish
Ukrainian
Vietnamese
Български
中文(简体)
中文(繁體)
Journal of Adhesive Dentistry 2010-Aug

Effect of water storage on the shear strength and fatigue limit of the reline resin bond to denture base resins.

Straipsnius versti gali tik registruoti vartotojai
Prisijungti Registracija
Nuoroda įrašoma į mainų sritį
Carlos Eduardo Vergani
Rosangela Seiko Seó
José Maurício Reis
Eunice Teresinha Giampaolo
Ana Cláudia Pavarina
Ana Lucia Machado

Raktažodžiai

Santrauka

OBJECTIVE

This study evaluated the effect of water storage (WS) on the shear bond strength (SBS) and shear bond fatigue limit (SBFL) between denture base and reline resins. In addition, a possible correlation between SBS and SBFL was evaluated.

METHODS

Two denture base (Lucitone 550-L and Acron MC-AC) and two reline resins (Ufi Gel Hard- UGH and Tokuso Rebase Fast-TR) were selected. Cylinders (20 x 20 mm) of each denture base resin were processed, and the reline resins were packed on the bonding surfaces using a split mold (3.5 x 5.0 mm). Specimens of each denture base-reline resin combination were subjected to shear forces (0.5 mm/min) until fracture. A staircase approach was used to determine the SBFL. Specimens were submitted to either 10,000 cycles (5.0 Hz) or until fracture. For both SBS and SBFL, specimens were tested after relining (control) and after 30 days of WS. Data (MPa) were analyzed with 2-way ANOVA and Tukey's tests (α = 0.05). To test for a possible correlation between the SBS and SBFL, a linear regression analysis was performed.

RESULTS

WS significantly increased (p < 0.05) the SBS of AC-TR and AC-UGH and the SBFL of AC-TR, AC-UGH and LUGH. After WS, UGH produced higher (p < 0.05) SBS than TR, regardless of the denture base resin used. Regardless of the experimental groups and the denture base resins used, UGH produced higher (p < 0.05) SBFL than TR specimens. A strong positive linear correlation (r(2) = 0.949) was observed between the SBS and SBFL.

CONCLUSIONS

Overall, UGH promoted the highest SBS and SBFL. WS increased the SBS and SBFL of the AC relined specimens. A positive correlation was observed between the two variables.

Prisijunkite prie mūsų
„Facebook“ puslapio

Išsamiausia vaistinių žolelių duomenų bazė, paremta mokslu

  • Dirba 55 kalbomis
  • Žolelių gydymas, paremtas mokslu
  • Vaistažolių atpažinimas pagal vaizdą
  • Interaktyvus GPS žemėlapis - pažymėkite vaistažoles vietoje (netrukus)
  • Skaitykite mokslines publikacijas, susijusias su jūsų paieška
  • Ieškokite vaistinių žolelių pagal jų poveikį
  • Susitvarkykite savo interesus ir sekite naujienas, klinikinius tyrimus ir patentus

Įveskite simptomą ar ligą ir perskaitykite apie žoleles, kurios gali padėti, įveskite žolę ir pamatykite ligas bei simptomus, nuo kurių ji naudojama.
* Visa informacija pagrįsta paskelbtais moksliniais tyrimais

Google Play badgeApp Store badge