Mongolian
Albanian
Arabic
Armenian
Azerbaijani
Belarusian
Bengali
Bosnian
Catalan
Czech
Danish
Deutsch
Dutch
English
Estonian
Finnish
Français
Greek
Haitian Creole
Hebrew
Hindi
Hungarian
Icelandic
Indonesian
Irish
Italian
Japanese
Korean
Latvian
Lithuanian
Macedonian
Mongolian
Norwegian
Persian
Polish
Portuguese
Romanian
Russian
Serbian
Slovak
Slovenian
Spanish
Swahili
Swedish
Turkish
Ukrainian
Vietnamese
Български
中文(简体)
中文(繁體)
Journal of the Mechanical Behavior of Biomedical Materials 2019-Oct

Air-abrasion using new silica-alumina powders containing different silica concentrations: Effect on the microstructural characteristics and fatigue behavior of a Y-TZP ceramic.

Зөвхөн бүртгэлтэй хэрэглэгчид л нийтлэл орчуулах боломжтой
Нэвтрэх / Бүртгүүлэх
Холбоосыг санах ойд хадгалдаг
Ana Cadore-Rodrigues
Catina Prochnow
Marília Rippe
Jivago de Oliveira
Sérgio Jahn
Edson Foletto
Gabriel Pereira
Luiz Valandro

Түлхүүр үгс

Хураангуй

This study assessed the fatigue performance (biaxial flexure fatigue strength), surface characteristics (topography and roughness) and structural stability (t-m phase transformation) of a Y-TZP ceramic subjected to air-abrasion using new powders (7% and 20% silica-coated aluminum oxide particles) in comparison to commercially available powders. Disc-shaped specimens were manufactured (ISO 6872-2015) and randomly allocated into four groups considering the air-abrasion materials: SiC: commercially available silica-coated aluminum oxide; AlOx: commercially available aluminum oxide; 7%Si and 20%Si: experimentally produced materials consisting of 7% and 20% silica-coated AlOx, respectively. Air-abrasion was executed by a blinded researcher (1 cm distance from the tip to the specimen surface, under 2.8 bar pressure for 10 s). The fatigue tests (n = 15) were performed by the staircase method under a piston-on-three-balls assembly. Topography and roughness assessments (n = 30) of abraded samples and fractography of failed discs were performed. The highest fatigue strength (MPa) was observed for 7%Si (887.20 ± 50.54) and SiC (878.16 ± 29.81), while the lowest fatigue strength for 20%Si (773.89 ± 46.44) and AlOx (796.70 ± 46.48). Topography analysis depicted similar surface morphology for all conditions. However, roughness (μm) was only statistically different between 7%Si (Ra = 0.30 ± 0.09; Rz = 2.31 ± 0.63) and SiC (Ra = 0.26 ± 0.04; Rz = 1.99 ± 0.34). Monoclinic phase grains appeared on Y-TZP surface in a similar content (≈11-12%) for the protocols. Fractography showed all failures starting on air-abraded surface/sub-surface defects from the tensile side. In terms of roughness, phase transformation and fatigue, the new 7% silica-coated aluminum oxide presented similar behavior to the commercially available powder. Increasing silica-coating concentration to 20% did not lead to a gentle air-abrasion protocol.

Манай facebook
хуудсанд нэгдээрэй

Шинжлэх ухаанаар баталгаажсан эмийн өвс ургамлын бүрэн мэдээллийн сан

  • 55 хэл дээр ажилладаг
  • Шинжлэх ухааны үндэслэсэн ургамлын гаралтай эдгэрэлт
  • Ургамлыг дүрсээр таних
  • Интерактив GPS газрын зураг - эмийн ургамлыг байршлаар нь тэмдэглэнэ (удахгүй)
  • Хайлттай холбоотой шинжлэх ухааны нийтлэлүүдийг уншина уу
  • Эмийн өвсийг үр нөлөөгөөр нь хайж олох
  • Мэдээллийн судалгаа, клиник туршилт, патентыг цаг тухайд нь сонирхож, зохион байгуул

Шинж тэмдэг эсвэл өвчний талаар бичиж, тус болох ургамлын талаар уншиж, өвслөг ургамлыг бичиж, өвчний эсрэг шинж тэмдгийг үзээрэй.
* Бүх мэдээлэл нь хэвлэгдсэн эрдэм шинжилгээний судалгаанд үндэслэсэн болно

Google Play badgeApp Store badge