Polish
Albanian
Arabic
Armenian
Azerbaijani
Belarusian
Bengali
Bosnian
Catalan
Czech
Danish
Deutsch
Dutch
English
Estonian
Finnish
Français
Greek
Haitian Creole
Hebrew
Hindi
Hungarian
Icelandic
Indonesian
Irish
Italian
Japanese
Korean
Latvian
Lithuanian
Macedonian
Mongolian
Norwegian
Persian
Polish
Portuguese
Romanian
Russian
Serbian
Slovak
Slovenian
Spanish
Swahili
Swedish
Turkish
Ukrainian
Vietnamese
Български
中文(简体)
中文(繁體)
Quintessence International 1998-Sep

In vitro evaluation of complex carbohydrate denture adhesive formulations.

Tylko zarejestrowani użytkownicy mogą tłumaczyć artykuły
Zaloguj się Zarejestruj się
Link zostanie zapisany w schowku
C G Tello
P Ford
A M Iacopino

Słowa kluczowe

Abstrakcyjny

OBJECTIVE

Acemannan, a complex mannose carbohydrate derived from the aloe vera plant, has an inherent stickiness/viscosity. Prototype Acemannan denture adhesive formulations were evaluated for pH changes, cytotoxicity to human gingival fibroblasts and adhesive strength in both dry and wet conditions.

METHODS

The denture adhesive formulations consisted of five combinations of Acemannan with varying concentrations of preservatives and two other formulations without preservatives. The pH of each formulation was measured over 24 hours. Assessment of cytotoxicity was accomplished using the in vitro, tetrazolium-based colorimetric assay on cultures of human gingival fibroblasts after exposure to the adhesive formulations for up to 24 hours. The adhesive strength was evaluated with a universal testing machine under initial dry conditions and after immersion in a constant-temperature water bath for up to 20 minutes.

RESULTS

Formulations 1 and 2 achieved and maintained pH values above 6.0 (the critical pH for hydroxyapatite dissolution) approximately 6 hours into the study. None of the prototypes demonstrated an initial pH above the critical pH. Formulations 1, 2, 3, and 5 exhibited significant cytotoxicity to human gingival fibroblasts over 24 hours. Formulations 4, 20:1, and 150:1 demonstrated minimal cytotoxicity. Formulation 1 exhibited the poorest adhesive strength, while the most viscous formulation (prototype 150:1) was by far the best performer. Generally, adhesive bond strengths for all prototypes were quite high and relatively stable over time in a wet environment.

CONCLUSIONS

To achieve the ideal adhesive in terms of strength, pH, and cytotoxicity, Acemannan formulation 150:1 should be adjusted to contain the preservative concentration of formulation 4 and have an initial pH value of 6.0 or higher.

Dołącz do naszej strony
na Facebooku

Najbardziej kompletna baza danych ziół leczniczych poparta naukowo

  • Działa w 55 językach
  • Ziołowe leki poparte nauką
  • Rozpoznawanie ziół na podstawie obrazu
  • Interaktywna mapa GPS - oznacz zioła na miejscu (wkrótce)
  • Przeczytaj publikacje naukowe związane z Twoim wyszukiwaniem
  • Szukaj ziół leczniczych po ich działaniu
  • Uporządkuj swoje zainteresowania i bądź na bieżąco z nowościami, badaniami klinicznymi i patentami

Wpisz objaw lub chorobę i przeczytaj o ziołach, które mogą pomóc, wpisz zioło i zobacz choroby i objawy, na które są stosowane.
* Wszystkie informacje oparte są na opublikowanych badaniach naukowych

Google Play badgeApp Store badge