Japanese
Albanian
Arabic
Armenian
Azerbaijani
Belarusian
Bengali
Bosnian
Catalan
Czech
Danish
Deutsch
Dutch
English
Estonian
Finnish
Français
Greek
Haitian Creole
Hebrew
Hindi
Hungarian
Icelandic
Indonesian
Irish
Italian
Japanese
Korean
Latvian
Lithuanian
Macedonian
Mongolian
Norwegian
Persian
Polish
Portuguese
Romanian
Russian
Serbian
Slovak
Slovenian
Spanish
Swahili
Swedish
Turkish
Ukrainian
Vietnamese
Български
中文(简体)
中文(繁體)
Dental Materials 2020-Jun

Influence of flavonoids on long-term bonding stability on caries-affected dentin

登録ユーザーのみが記事を翻訳できます
ログインサインアップ
リンクがクリップボードに保存されます
Andrés Dávila-Sánchez
Mario Gutierrez
Jorge Bermudez
María Méndez-Bauer
Bruna Hilgemberg
Salvatore Sauro
Alessandro Loguercio
Cesar Arrais

キーワード

概要

Objectives: To evaluate the effect of experimental dentin pre-treatment solutions formulated with different flavonoids on microtensile bond strength (μTBS), nanohardness (NH) and ultra-morphological characteristics of artificial caries-affected dentin (CAD) bonded using a universal bonding system.

Methods: A microbiological method was used to create an artificial CAD in 91 human molars. Five experimental pre-treatment solutions were created using the following flavonoids: quercetin (QUE); hesperidin (HES); rutin (RUT); naringin (NAR), or proanthocyanidin (PRO). A placebo solution (PLA) with no flavonoids added was also evaluated. The flavonoids or placebo solutions were applied to the CAD prior to the application and photoactivation of a universal adhesive (Scotchbond Universal, 3M Oral Care). A control group (CON), in which only the bonding agent was applied without any flavonoid solution, was also evaluated. A 3-mm-thick block of resin composite (Opallis, FGM) was built up on the flat bonded CAD surfaces and was light-cured following the manufacturer's instructions. Specimens were sectioned to obtain resin-dentin slices and sticks (cross-sectional area of 0.8 mm2). The μTBS, NH, and confocal ultramorphology analysis of resin-dentin interface was evaluated at 24 h and after thermo-cycling aging (25,000 cycles). The results were analyzed using 2-way ANOVA followed by Bonferroni's post hoc test (pre-set α = 0.05).

Results: The specimens from groups QUE, NAR, and RUT presented greater μTBS values than those from CON group (p<0.05). Specimens from some of these experimental groups presented greater nanomechanical properties (p<0.05), and no morphological degradation at the resin-dentin interface after aging.

Significance: The use of exogenous cross-linkers as dentin pre-treatment before bonding procedures may represent a suitable strategy to improve the longevity of universal adhesive systems applied to caries-affected dentin.

Keywords: biomaterials; bonding; caries; nanoindentation; universal adhesives.

Facebookページに参加する

科学に裏打ちされた最も完全な薬草データベース

  • 55の言語で動作します
  • 科学に裏打ちされたハーブ療法
  • 画像によるハーブの認識
  • インタラクティブGPSマップ-場所にハーブをタグ付け(近日公開)
  • 検索に関連する科学出版物を読む
  • それらの効果によって薬草を検索する
  • あなたの興味を整理し、ニュース研究、臨床試験、特許について最新情報を入手してください

症状や病気を入力し、役立つ可能性のあるハーブについて読み、ハーブを入力して、それが使用されている病気や症状を確認します。
*すべての情報は公開された科学的研究に基づいています

Google Play badgeApp Store badge